Basic Compounds for Superalloys

Mechanical Properties de

Éditeur :

Elsevier


Paru le : 2018-06-29

eBook Téléchargement , DRM LCP 🛈 DRM Adobe 🛈 ebook sans DRM
Lecture en ligne (streaming)
205,72

Téléchargement immédiat
Dès validation de votre commande
Image Louise Reader présentation

Louise Reader

Lisez ce titre sur l'application Louise Reader.

Description
Basic Compounds for Superalloys: Mechanical Properties explores the mechanical properties of the iron group based intermetallic compounds that are the basis of super-alloys. Chapters explore tensile tests and compressive stress and hardness and provide detailed considerations that are devoted to time dependent deformation, namely creep and cyclic deformation. In addition, a discussion of the nano-crystalline L12 and B2 structures and their mechanical properties is included. Fracture and failure of these materials in both macro and nano-iron based compounds is also considered. This book is ideal for engineers, scientists and technical personnel who work in materials engineering, materials science, and mechanical and chemical engineering. - Provides an in-depth focus on the mechanical properties of Fe- superalloy materials - Includes a discussion of the static, time dependent and cyclic deformation properties of macro- and nano materials - Reviews how superalloy materials behave under a variety of 'in-service' environments and conditions
Pages
624 pages
Collection
n.c
Parution
2018-06-29
Marque
Elsevier
EAN papier
9780128161333
EAN PDF
9780128162323

Informations sur l'ebook
Nombre pages copiables
62
Nombre pages imprimables
62
Taille du fichier
45701 Ko
Prix
205,72 €
EAN EPUB SANS DRM
9780128162323

Informations sur l'ebook
Prix
205,72 €

Suggestions personnalisées